- Recommended settings for PETG? (re: OVERTURE brand PETG)
I'm using an Ender 3 (upgraded to Capricorn PTFE tubing and other upgrades) and I'd like to try printing PETG More specifically, I've purchased a roll of the OVERTURE PETG The manufacturer recommends: Nozzle Temp: 230 - 250 Bed Temp: 80 - 90
- What Are the Optimal Settings for Overture PETG? (Detailed)
Here are the optimal settings for Overture PETG, as recommended by the manufacturer: Nozzle (Print) Temperature – 230 to 250 degrees Celsius Bed Temperature – 80 to 90 degrees Celsius
- Overture PETG settings - Bambu Lab Community Forum
Your petg flow should be around 95 to 98 range with most petg filaments set it to 96 and run a calibration flow test PA 0 02 to 0 05 range should be in Also do all your calibrations on a smooth bed plate
- The PETG Print Settings for Perfect Results - All3DP
Find the perfect PETG print settings for your needs by adjusting temperature, stringing, print speed, and retraction settings!
- PETG Print Settings: Temperature, Speed, and Retraction - CREALITY CLOUD
PETG generally prints best within a temperature range of 220°C to 260°C Many experts recommend starting with a nozzle temperature of 230°C for the first layer and 240°C for the subsequent layers
- I Finally Got Overture PETG To Print : r BambuLab - Reddit
Looking around online, many suggest 4-10, usually around 8 or 10 for the max speed setting for PETG First layer is missing filiment It's either not adhering, or you're printing too fast
- Looking for the best settings for printing with PETG
You’ll likely get better results if you use a PETG filament that’s rated for high speed printing (300mm sec minimum, but generally the higher the speed rating the better) The same for other filament types also, if you can find it
- How to 3D Print PETG Filament Like a Pro – Ultimate Guide FAQ
To 3D print PETG, you should use a printing temperature between 235-250°C and a bed temperature between 70-100°C for the best results Your cooling fan should be at 100%, with a print speed of 40-60mm s Also, PETG absorbs moisture easily so, keep it dry in an airtight container when not in use
- PETG First Layer Settings using Overture PETG - Prusa3D Forum
I'm using the generic PETG settings in PrusaSlicr which uses a temp of 230 The parts printed fine and look excellent except the first layer of most parts has a very smooth finish on one portion and visible lines on the rest that you can feel when you run a fingernail across them
|
|